Digital prototyping specialist Protolabs has launched a new 3D printing material for its metal laser sintering process – cobalt chrome superalloy. The UK-based company believes the heat, wear, and corrosion resistant material will disrupt a number of industries including oil and gas where customized cobalt chrome parts were not previously possible. Andrea Landoni, 3D printing […]